douglas fur on thu 6 oct 11
Mike how 'bout this re-write?
I'm trying to come up with a fair price for insulating F.B. a friend is
willing to sell. As a deal between friends can lead to hard feelings I'm
throwing this out to you.
My friend bought the brick from other friends in about 1985-88.
The kiln *they're from* was built in 1976-78 and was fired maybe 40 to 75
times ^10 reduction.
The brick are APGreen 2300 and 2600 insulating fire brick.
They have been stored in a dry but unheated barn.
On Thu, Oct 6, 2011 at 1:14 PM, Mike Gordon wrote:
> Douglas, DEFINITELY not $3.00 a piece. Were these bricks in the kiln? tha=
ts
> not clear to me. Mike Gordon
>
> On Oct 6, 2011, at 11:32 AM, douglas fur wrote:
>
> Clayarters
>> I'm trying to come up with a fair price for insulating F.B. a friend is
>> willing to sell. As a deal between friends can lead to hard feelings I'm
>> throwing this out to you.
>> My friend bought the brick from other friends in about 1985-88.
>> The kiln was built in 1976-78 and was fired maybe 40 to 75 times ^10
>> reduction.
>> The brick are APGreen 2300 and 2600 insulating fire brick.
>> They have been stored in a dry but unheated barn.
>>
>> What would you expect to pay/ea.-$.50, $.75, $1.50, $3.00?
>>
>> Thanks
>> DRB
>> Seola Creek
>>
>>
>
| |
|