search  current discussion  categories  glazes - crystalline 

a new crystalline glaze test photo

updated tue 22 nov 11

 

Brad Sondahl on mon 21 nov 11


I've added to an old web page I'd put up years ago on how to hybridize
glaze tests and multiply your results as a quick method to solving glaze
problems. I've put up a photo showing 44 results from 9 glaze tests and the
qualitative differences resulting from doubling or leaving out some of the
glaze chemicals. This is the direct link to the page:
http://sondahl.com/glazetest.html#2011
If you want to learn more about the process it's described above the target
in the page.
Brad Sondahl
http://www.sondahl.com