search  current discussion  categories  techniques - majolica 

majolica clay

updated mon 2 feb 98

 

Jack Ward on fri 30 jan 98

In the east Highwater clay sell Stan`s Red developed for majolica.
Highwater Clay
POB18284
238 Clingman Ave.
Ashville.NC 28814
704 252 6033
fax. 704 253 3853
e-mail WIGHWATERC@AOL.COM

Jack Ward on sat 31 jan 98

Sorry wrong e-mail
Highwater e-mail HIGHWATER@AOL.COM

> ----------------------------Original
> message----------------------------
> In the east Highwater clay sell Stan`s Red developed for majolica.
> Highwater Clay
> POB18284
> 238 Clingman Ave.
> Ashville.NC 28814
> 704 252 6033
> fax. 704 253 3853
> e-mail WIGHWATERC@AOL.COM

Carol Tague on sun 1 feb 98

In the south Florida Clay Art Co. sells Highwater Clay, Stan's Red
included. Really great prices too! Carol @Florida Clay Art Co.
1-800-211-7713 1645 Hangar Rd. #103, Sanford, FL 32773.

At 09:57 AM 1/30/98 EST, you wrote:
>----------------------------Original message----------------------------
>In the east Highwater clay sell Stan`s Red developed for majolica.
>Highwater Clay
>POB18284
>238 Clingman Ave.
>Ashville.NC 28814
>704 252 6033
>fax. 704 253 3853
>e-mail WIGHWATERC@AOL.COM
>
>