Lili Krakowski on fri 9 mar 12
Don't call the white-coated team with the nice net!=3D20
I need, yes, need, recipes for some really really blistery c. 6 glazes. =
=3D
This for some tests I want to run regarding--you guessed--blisters. =3D
It is easier to ask than to look through 60 years worth of notes.
Please send off list.
Thank you.
Lili Krakowski
Be of good courage
Bonnie Staffel on sat 10 mar 12
Lili, I added find silicon carbide to the glaze and got great bubbling wher=
e
I could smash the blisters to have open craters. No recipe, just do it
Bonnie
http://webpages.charter.net/bstaffel/