casting

updated thu 15 mar 12

 

Rimas VisGirda on wed 14 mar 12


I did a residency at Kohler many years ago. There they taught me to wet onl=
y the inside of the mold with a heavily water laden sponge. This starts the=
water migration from the inside to the outside. -Rimas