DJ Brewer on tue 1 may 12
For those who do electric kiln firing, what are your favorite books and
tips for getting creative glaze results out of your electric kiln?
thanks for your responses!
DJ
William & Susan Schran User on tue 1 may 12
On 5/1/12 2:43 PM, "DJ Brewer" wrote:
>For those who do electric kiln firing, what are your favorite books and
>tips for getting creative glaze results out of your electric kiln?
Top of my list would be Mastering Cone 6 Glazes by Hesselberth & Roy.
Bill
--
William "Bill" Schran
wschran@cox.net
wschran@nvcc.edu
http://www.creativecreekartisans.com
>
| |
|