Deborah Thuman on sun 27 may 12


Not knowing what I was doing, I added some mason stain to terra sig. I =3D
did get color, but not the intensity I desired. I just took some of the =3D
class white terra sig and added some mason stain and stirred like crazy. =
=3D
No, I did not measure.=3D20

I spent a lot of time in my early classes wondering what if - and then =3D
went and tried it. I had some flops, like the time I tried reduction =3D
firing for ^04 and had some great successes like the time I tried =3D
reduction firing for ^6. The most important lesson I learned is: give it =
=3D
a shot and see what happens.=3D20

Deb Thuman