KathysPottery@AOL.COM on sat 16 jun 12
Hi, I have lost my recipe for paper clay to repair cracks in bisque ware. I
got it a long time ago from someone on this site, and am hoping someone
has it.
Also, does anyone know of something that could be put on the bottom of a
vase that cracked in the bottom in the glaze firing that would make it
waterproof? The crack did not go all the way through in this cone 5 fired p=
iece,
but it still leaks.
Thanks,