we too make the hook with a neddle nose plier.
kerry was doing that with all of her kilns when
we rebuilt and did the itc thing.
it is so easy...and it works much better.
i don't think we have to make a video.
make a hook on the end of the element pin
with a needle nose plier.
grab it with the plier and push.
add extra, they work and save the elements from
drooooping. get them in there tight.
(then spray the entire thing with itc 100. and you
won't be changing elements for a long time.)