search  current discussion  categories  kilns & firing - gas 

gas controls/regulators

updated fri 20 feb 98

 

Mel Jacobson on thu 19 feb 98

In dealing with Dannon's kiln we have run into problems getting
the proper high pressure regulators....we are going from 10 pounds
of pressure and want to regulate it to maybe 7 pounds. I have found
the proper company thanks to my plumbing contractor/supply house.
\ they use:

Maxitrol
23555 Telegraph Rd.
Southfield, MI
48037
phone 248.356.1400
fax 248.356.0829

they have all kinds of gas regulators....they have indicated that
they can interchange natural gas and propane with all of their
regulators.

we are going to use a 1/2 inch in...10 pounds...regulated to 5-7
pounds to the burners.

a special thanks to marc ward and vince who have been
digging on this project.

mel.mn

http://www.pclink.com/melpots