Rhodes Black: ^9/10 reduction:

Albany Slip 75
Neph Syenite 20
Cobalt Oxide 5

(I typically subtitute with cobalt carb and use 1.5 times more of the carb
than the oxide) Also if you know sources and pricing for the True Albany
Slip, I would be interested to know, however, I don't think that it is
worth what the owners charge for it. TIA...Marshall

101 CLAYART MUGS (Summer 1998)
2ND ANNUAL CLAYARTERS' GALLERY - NAPLES, MAINE (Summer 1998)
E-MAIL ME FOR APPLICATIONS
http://fmc.utm.edu/~dmcbeth/cag/naples.htm

Celia & Marshall Talbott, Pottery By Celia, Route 114, P O Box 4116,
Naples, Maine 04055-4116,(207)693-6100 voice and fax,(call first)
Clayarters' Live Chat Room, Fri & Sat Nites at 10 PM EDT & Sun at 1 PM EDT
http://webchat12.wbs.net/webchat3.so?Room=PRIVATE_Clayarters
---------------------------------------------------------------------

the cat lady on sat 21 feb 98

At 07:48 AM 2/19/98 EST, you wrote:
>----------------------------Original message----------------------------
>I don't know how much difference there is between the three but would be
>curious to know. The glaze that I would be making up is the following:
>
>
>Rhodes Black: ^9/10 reduction:
>
>Albany Slip 75
>Neph Syenite 20
>Cobalt Oxide 5
>
>(I typically subtitute with cobalt carb and use 1.5 times more of the carb
>than the oxide) Also if you know sources and pricing for the True Albany
>Slip, I would be interested to know, however, I don't think that it is
>worth what the owners charge for it. TIA...Marshall
>
Easiest receipe for black I ever used:

100 Albany slip
10 Cobalt ox

Have also done this with alberta slip, also a nice black