John Baisch on tue 3 mar 98
Hello all,
Playing with Glazes and wanted to experiment with Randy's
Green a little. I've been firing
Randy's Green from Ruthann's soda firing book in cone 10
salt reduction. I'd like to try firing a version of Randy's
green in both Cone 5-6 oxidation no-salt and also in ^5-6
reduction. Has anyone had any experience with this and/or
has a variation of the recipe that will work?
Any help would be grealty appreciated,
Thanks much,
John Baisch
| |
|