Arturo M DeVitalis on sat 28 mar 98

My supplier, Refractory Maintainance, Williamson, NY tells me that
Thermal Ceramics took over AP Green IFB manufacturing in January of this
year and the listed specs for G23 and G26 that were given to Steve are
not accurate, ie, G23 have a much better thermal conductivity @2000F than
G26. For more info go to the Thermal Ceramics web page. Also the method
used to produce"Greenlites" is no longer being used and now all current
bricks are dimensionally true.