Foresthrt on wed 1 apr 98
Please try to always post cones with glaze recipes!
some of us may not know what is familiar to others-
Ron Roy's Floating Blue Rev. 1 cone????
Cobbeldi Floating Blue Rev. 1 cone???
Mary
Gregory D Lamont on thu 2 apr 98
Mary,
Sorry to not post the cones for these glazes. Theyre both for cones 5-6
fired in an electric kiln.
I've run tests on both and they both work well.
Greg
At 08:54 AM 4/1/98 EST, you wrote:
>----------------------------Original message----------------------------
>Please try to always post cones with glaze recipes!
>some of us may not know what is familiar to others-
>
>Ron Roy's Floating Blue Rev. 1 cone????
>Cobbeldi Floating Blue Rev. 1 cone???
>
>Mary
>
| |
|