To the person asking about glazing and bisqueing at the same time:

I got your question on clayart. I teach at a high school and sometimes the
students use a ^06 clear for slip decorated work. To save time and $ many
times I will bisque and glaze fire this clear glaze with no problems to
either the glaze ware or the bisque ware.