Anthony G Allison on mon 6 apr 98
Hello Fellow Potters,
Does anyone know where I can obtain some Avery kaolin? Where does it come
from and what's the skinny on it?
Tony
Isn't spring the greatest?
Gari Whelon on tue 7 apr 98
Hi Tony
If you find any please let me know.
The last I heard the mine had run out and its no longer available.
I'd love to find and try some, I've seen the results of it and they are
quite wonderful.
I've been using Helmer Kaolin for flashing and it works well either as a
slip or a part of the clay body.
Gari Whelon
Nanaimo, B.C.
>----------------------------Original message----------------------------
>Hello Fellow Potters,
>
>Does anyone know where I can obtain some Avery kaolin? Where does it come
>from and what's the skinny on it?
>
>Tony
>
>Isn't spring the greatest?
>
>
Anthony G Allison on wed 8 apr 98
Hi Gari,
What effects do you get and where do you obtain Helmer Kaolin?
Thanks,
Tony
At 07:57 AM 4/7/98 EDT, you wrote:
>----------------------------Original message----------------------------
>Hi Tony
>
>If you find any please let me know.
>
>The last I heard the mine had run out and its no longer available.
>
>I'd love to find and try some, I've seen the results of it and they are
>quite wonderful.
>
>I've been using Helmer Kaolin for flashing and it works well either as a
>slip or a part of the clay body.
>
>Gari Whelon
>Nanaimo, B.C.
>
>>----------------------------Original message----------------------------
>>Hello Fellow Potters,
>>
>>Does anyone know where I can obtain some Avery kaolin? Where does it come
>>from and what's the skinny on it?
>>
>>Tony
>>
>>Isn't spring the greatest?
>>
>>
>
Gari Whelon on mon 13 apr 98
Hi Tony
sorry for the delay, I've been way from the computer.
effects? nice warm flashing in wood fire, browns through oranges to reds
when used as a slip with neph sy 80/ 20 or 85/15
Archie Bray has it, My supplier orders it from them, I also get it at
Georgies whenever I'm down in Portland.
What are you looking at using for.
Gari
>----------------------------Original message----------------------------
>
>Hi Gari,
>
>What effects do you get and where do you obtain Helmer Kaolin?
>
>Thanks,
>
>Tony
>
>
>
>
>
>
>
>
>
>
>At 07:57 AM 4/7/98 EDT, you wrote:
>>----------------------------Original message----------------------------
>>Hi Tony
>>
>>If you find any please let me know.
>>
>>The last I heard the mine had run out and its no longer available.
>>
>>I'd love to find and try some, I've seen the results of it and they are
>>quite wonderful.
>>
>>I've been using Helmer Kaolin for flashing and it works well either as a
>>slip or a part of the clay body.
>>
>>Gari Whelon
>>Nanaimo, B.C.
>>
>>>----------------------------Original message----------------------------
>>>Hello Fellow Potters,
>>>
>>>Does anyone know where I can obtain some Avery kaolin? Where does it come
>>>from and what's the skinny on it?
>>>
>>>Tony
>>>
>>>Isn't spring the greatest?
>>>
>>>
>>
>
>
| |
|