search  current discussion  categories  glazes - traditional iron glazes 

fwd: re: oribe and shino glazes for a wood kiln

updated sat 18 apr 98

 

Dannon Rhudy on fri 17 apr 98


As an addendum to Doug's note, I have tried this glaze. On
stoneware, slightly matt, more or less opaque, crystals, like
it a lot. On porcelain, translucent, glassy, strong tendency to
blush pink. Don't like it so much on porcelain, seems - vague,
somehow. But that may be just one of the different kiln/different
place glitches. Also, in mine, used tri-calcium instead of
real bone ash, because that is what I had.

Dannon Rhudy
potter@koyote.com


----------------------------Original
message----------------------------
Les,

.......Here is an Oribe glaze......

Oribe Green (attributed to David Shaner) cone 9-11 reduction

29.3 Custer Feldspar
24.0 Silica
21.2 Whiting
7.4 Talc
11.9 EPK (Kaolin)
1.0 Bone Ash
1.0 Bentonite
5.2 Copper Carbonate