John Britt on tue 21 apr 98

Black Mtn liner Glaze
Soda Spar 50
Flint 25
Whiting 12.5
Kaolin 12.5

Val's Blk

Custer spar 20
Soda spar 20
Dlint 20
Dolomite 15
Talc 13
Om-4 10
Whiting 2
Cobalt Ox 3
RIO 3
Manganese Dio 2
Chrome 1

You should buy Val's book!
--
Thanks,

John Britt claydude@unicomp.net