2600 new apgreen bricks for sale

updated thu 23 apr 98

 

ThePottery on wed 22 apr 98

There are some ins soft AP Green 2600 bricks still in their boxes for sale
near Johnson City Tenn.....!!!!But they are #2 splits....4 1/2 by 9 by 2
inches (a standard brick is 2 1/2 inches thick) for !.00 each. Good buy if
you can build your entire kiln with them. Contact Brad Thompson, Thompson
Metals, Bluff City Tenn, 423-538-6137.