Mudnjoy on thu 23 apr 98
In a message dated 98-04-10 09:23:07 EDT, you write:
> ---------------------------Original message----------------------------
> Tested a clear glaze at ^6 ox that was posted by Michelle Lowe. It was
nice
> and clear and no crazing. The numbers didn't add up to 100 and I'm
> wondering
> if I'm missing something, even though it turned out well. Nice and simple
> formula.
> Anyone?
>
> Gerstley Borate 25
> Flint 15
> Kaolin l5
>
Has anyone tried this single fire? Joy in Tucson
| |
|