search  current discussion  categories  kilns & firing - flues & venting 

kiln venting information

updated sat 25 apr 98

 

MLCeramics on thu 23 apr 98

Does anyone know of any good articles on why one should vent an electric kiln?
I would appreciate any information that you might know of that addresses the
benefits of venting and the health hazards of not venting. Thanks, Meg Levine

The Kiln Guy on fri 24 apr 98

> I would appreciate any information that you might know of that addresses
the
> benefits of venting and the health hazards of not venting. Thanks, Meg
Levine

Hi Meg,
Try contacting the Orton Ceramic Foundation @ 800-999-5442. They have done
extensive testing for their downdraft vent system & have created some good
literature on the subject.
Chris @ Euclid's Kilns and Elements
1-800-296-5456
Web Site: http://www.euclids.com
E-Mail: mail@euclids.com

jjcat on fri 24 apr 98

Meg,

Orton has a great deal of literature so does Vent-A-Kiln should you need
their telephone # e-mail us.

If you are considering purchasing either after you decide check us out for
the a quote on either.

Kiln-Ray Services

Ask for Joe

At 07:40 AM 4/23/98 EDT, you wrote:
>----------------------------Original message----------------------------
>Does anyone know of any good articles on why one should vent an electric kiln?
>I would appreciate any information that you might know of that addresses the
>benefits of venting and the health hazards of not venting. Thanks, Meg Levine
>
>