Linda Blossom on thu 23 apr 98

Joy wrote:
=22I hope someone else gives you the chemical info, sounds interesting. All=
of
the chemicals you list will affect oxide =26 slip treatments of leather =26
greenware =26 most likely will eliminate any single fire glazing. =22

This is not meant as an attack on Joy, but I have a problem with people =
making
statements based on what they think would happen although they have no
experience in what is being discussed. Joy is certainly not the first =
person to
do this, and I may even have done it myself, but I have tried to discipline
myself to respond only when the subject is something I have had a lot of =
direct
experience with. WD 40 in the extruder barrel or anywhere else, will not
affect being able to single fire glazing. I single fire exclusively and use
wd-40 in the barrel, have done so every time I have extruded, and have also =
used
it in other methods and tools with no ill effect.


Linda Blossom
2366 Slaterville Rd.
Ithaca, NY 14850
6075397912
www.artscape.com
blossom=40lightlink.com