Andrew B. Gardner on mon 11 may 98
Hi folks!
I'm a potter working at the Craft Students League in NYC. We've been
having a problem with our white porcelin (cone 6) slip literally slipping
off during glaze firing. We're currently using Jack Wolfe's
cone 6 Brooklyn Museum mix clay as a body. Anybody got any thoughts, or
know of a good white slip for application to greenware on our clay body?
Andy
| |
|