I am using "Mather Stoneware" a prepared clay, I am having trouble with
crazing. My current glaze is: Neph Sy 1300, Silica 1100, epk 1000, and
gertsley borate 1600. I fire to cone 6 oxidation. Does anyone have a
suggestion or better yet have a receipe for another clear gloss cone 6
glaze?? Where can I get receipes for cone 6 oxidation firing??
I appreciate your thoughts,
Gloria
Ron Wright on tue 19 may 98
Try the AACC#2 glaze on my web page. It's very similar to yours. I've
used it on at least 12 differant clay bodies never had it craze.
Ron Wright
3 Dogs Pottery - Chicago
http://www.concentric.net/~wrright
BBC wrote:
>
> ----------------------------Original message----------------------------
> I am using "Mather Stoneware" a prepared clay, I am having trouble with
> crazing. My current glaze is: Neph Sy 1300, Silica 1100, epk 1000, and
> gertsley borate 1600. I fire to cone 6 oxidation. Does anyone have a
> suggestion or better yet have a receipe for another clear gloss cone 6
> glaze?? Where can I get receipes for cone 6 oxidation firing??
> I appreciate your thoughts,
> Gloria
| |
|