I have a question about low fire clay, I have some cone 06-04 clay, at what
come temperature I should bisque fire the pot?
thanks in advance, Welson
paul wilmoth on sat 30 may 98
Welson,
I use two different low-fire bodies. The white talc body I bisque
to 01 and glaze fire to 04. The red terra cotta body I glaze and bisque
fire to 04. The higher bisque temps. help out greatly with many types of
glaze problems, especially crazing and pinholes.
peace - Paul