search  current discussion  categories  forms - tiles 

tilemakers questions

updated sat 30 may 98

 

Susan Schultz on fri 29 may 98

Kristin-
I make tiles and large 3 -dimensional murals and have used
Miller 10T (now from Laguna) for many years-I wedge in fine grog when
I need to (rarely). I dry VERY slowly, and check drying a lot,
and have little problems with warping. My mural sections are often
large. I had glazing problems with #10 Miller Clay, so don't know if
if I'd recommend 10G (with grog).

Susan Schultz
Stonington, Ct.