Beth Yeatman Spindler on fri 19 jun 98
Nathan.......(sorry, don't have your e-mail address)
Not sure where you live, but if you are anywhere near Blowing Rock/Lenoir, NC
area, you can see a groundhog kiln at Bolick Family Pottery. A kiln openng
and bluegrass festival is scheduled for Saturday, June 27 from 8 a.m. to 4
p.m. at the pottery....located between Blowing Rock and Lenoir...Highway
321....Blackberry Road (off 321 to Bolick Road....directional signs will get
you there)....Lula and Glen Bolick can be reached at
704-295-3862........mailing address: Rt. 8, Box 285, Lenoir, NC 28645.
Heading there myself on Friday, June 26.........don't want to miss a minute of
things on Saturday..........
Beth in Blue Ridge Mtns Foothills of VA
P. S. Traditions Pottery, located next to Bolick Pottery will also be
participating in the kiln opening.......a family affair......:) And Glen
Bolick is the national hollering champion of the U. S......so celebrities will
be on hand as well!!!! :)) :))
Bill Downs on sat 20 jun 98
Nathan
If you haven't already, check out Studio Potter Dec. 97, "Adapted Groundhog
Kiln"
by Vernon and Pam Owens. The kiln is in Seagrove N.C..Limited plans are
included
in the article.