I was rather surprised at hearing that folks are having problems
with the Reward velvets UGs. I've been using them for several years now
and I love 'em ! I've been using them with Duncan GL lead free clear.
fired to cone 4/6 (one good brushed on coat does the trick)...never had a
problem with crawling.

(according to the color chart sheet) look too good to be true !