search  current discussion  categories  glazes - misc 

longivity...glazes

updated mon 6 jul 98

 

Tracey Dobbins on sun 5 jul 98

-------------------
Am wondering just how long a glaze, that's say around 50=25 gertsley borate,=
can
be mixed up without going bad. I've heard it has a short life once mixed up
with water. Would the time frame be different for thicker, pastey glazes
compared to thin, skim milk kinda glazes? What's the longest anyone has =
noticed
success with wet glaze mixtures?

This info will surely help many of us to not waste costly glaze materials.
Thanks to all the glaze gurus for pondering here...