search  current discussion  categories  wanted/for sale - misc 

canvas covered work area

updated wed 15 jul 98

 

Caryl W. on tue 14 jul 98

I use a canvas covered board for a wedging/work area for red clay, and a
canvas covered table for the same when I'm using light colored clay, so
there is no contamination. I find that to get a good fit when you're
stretching the canvas, I wet it thoroughly first and then stretch it.It
shrinks up slightly when it dries, which makes it nice and tight and
much easier to scrub clean after use.If you clean it immediately after
use with a hard brisle brush and water, it comes really clean so dust
isn't really a factor.

Caryl