search  current discussion  categories  materials - misc 

pioneer kaolin?? epk kaolin???

updated thu 23 jul 98

 

nlstraker@juno.com on sun 19 jul 98

X-Juno-Line-Breaks: 0-4


[Moderator's Note: you can look up the answers to this kind of thing using
the CeramicsWeb Material Analysis database.]

Hey Folks,

Can anyone tell me if Pioneer and EPK are the same??

Thanks in advance! Norm! 8^o

_____________________________________________________________________
You don't need to buy Internet access to use free Internet e-mail.
Get completely free e-mail from Juno at http://www.juno.com
Or call Juno at (800) 654-JUNO [654-5866]

Tony Hansen on mon 20 jul 98

The two have similar chemistries but are somewhat different
physically. Pioneer Kaolin is not as white burning as EPK, it is
not as consistent from batch to batch, and it tends to flash with
a greyish coloration. EPK is better in glazes because it tends
to gel (flocculate) the slurry. Pioneer is a little more plastic
in clay bodies. These clays come from two different companies,
one is a lot more consciencious toward the ceramic community
than the other, I won't say which.

--
T o n y H a n s e n thansen@digitalfire.com
Don't fight the dragon alone http://digitalfire.com
Calculation/Database Software for Ceramic Industry

Norm Straker on tue 21 jul 98

Hi Tony,

The reason I was asking was because of your cone 6 matte glaze. I have
about 100 pounds of EPK that I would like to be able to use. Will EPK be
good to use??

Thanks for all your help and especially the time you put in on your Glaze
web pages. I love them!

Norm! 8^o

_____________________________________________________________________
You don't need to buy Internet access to use free Internet e-mail.
Get completely free e-mail from Juno at http://www.juno.com
Or call Juno at (800) 654-JUNO [654-5866]

Tony Hansen on wed 22 jul 98

EPK is the only kaolin I use in glazes. It gels the glaze better
than anything I have seen. If you can get 20% or better EPK into
a glaze it often glides on with no drips into an even layer that will
stick and stay even on the densed bisque ware.

--
T o n y H a n s e n thansen@digitalfire.com
Don't fight the dragon alone http://digitalfire.com
Calculation/Database Software for Ceramic Industry