Edouard Bastarache on sun 2 aug 98
Hello all,
i think recently someone asked for the chemical analysis of this clay;here
it is:
SIO2.........59.70%
AL2O3......10.87%
FE2O3......14.65%
TIO2.........0.67%
CAO.........0.27%
MGO........0.75%
MNO........3.40%
K2O.........2.04%
NA2O.......O.12%
L.O.I.........7.46
LATER,
Edouard Bastarache
edouardb@sorel-tracy.qc.ca