search  current discussion  categories  techniques - slips 

dry wall - not for slip!!

updated sun 9 aug 98

 

Janet or Michael Francoeur on sat 8 aug 98

We're talking about drying tiles that you have rolled! Good luck - janet

----------
> From: Ardis Bourland
> To: CLAYART@LSV.UKY.EDU
> Subject: dry wall
> Date: Friday, August 07, 1998 2:09 PM
>
> ----------------------------Original message----------------------------
> I am interested in your references to using dry wall. I tried drying
some
> slip on it and the top layer of paper peeled off onto the clay. Ugh. I
must
> be doing something wrong???
> Ardis