rivkin toby on fri 31 jul 98
Thanks to everyone who responded to my lin shelf questions! Next question:
I tend to fire both electric and gas up to cone 10. What is the difference
between Cordierite, Mullite, and Silicon Carbide shelves?
Toby Rivkin
J. D. Walker on sat 1 aug 98
toby
from a working stand point.
good - Cordierite. Better - Mullite, Best - Silicon Carbide, THE VERY
BEST - Advancer Shelves from Fire Brick Supply.
-----Original Message-----
From: rivkin toby
To: CLAYART@LSV.UKY.EDU
Date: Friday, July 31, 1998 3:06 PM
Subject: Mullite vs Cordierite vs Silicon Carbide
----------------------------Original message----------------------------
Thanks to everyone who responded to my lin shelf questions! Next question:
I tend to fire both electric and gas up to cone 10. What is the difference
between Cordierite, Mullite, and Silicon Carbide shelves?
Toby Rivkin
| |
|