David Hendley on mon 27 jul 98
At 04:01 PM 7/26/98 -0400, you wrote:
> 1. Is it worth it to try to sand or otherwise remove the kiln wash
>from the bottom of the shelves that aren't warped? What would you use to
>do this? One suggestion was a silicon carbide disk attached to a power
>drill. Any other ideas?
>
Sandblasting.
I would consider it $$ well spent to drop off the shelves at the
sandblasing place and return with clean shelves.
David Hendley
Maydelle, Texas
| |
|