David Orser on sun 1 nov 98
---------- Forwarded message ----------
Date: Fri, 30 Oct 1998 15:22:34 -0500 (EST)
From: David Orser
To: kpotter@ufl.edu
Subject: aventurine glaze
had this one in the file, never tried it.... ???
borax 46.00
strontium carb 1.96
boric acid 3.32
epk 1.71
flint 47.01
riox 17.82
also, ithink i saw someone do something simple like 50/50
rutile/gerstley borate and get some wacky crystalline thing...
p.s. this is rated for 05-07.. try adding rutile or titanium
bet it's runny as hell, good luck
| |
|