john eden on tue 24 nov 98
I would appreciate it if someone could give me details on the following
bricks, maker, temp, etc..
Firebrick "HI - HEAT"
Firebrick "S - I DP
Thanks in advance, cheers, John.
John Eden
Hudson, Quebec, J0P 1H0, Canada
Tel. # 514-457-6610 ext. 395 (office)
Tel. # 450-458-7097 (home)
e-mail> john.eden@johnabbott.qc.ca
Donovan Palmquist on thu 26 nov 98
In response to your inquiry about identification of "HI HEAT" & "S - I DP
hard firebricks. The HI - HEAT is a Dixon -Ticonderoga high duty
hardbrick, the S - I DP is also a high duty hard firebrick that is
manufactured using the "dry press" method.
Hope this answers your question.
Donovan Palmquist
Master Kiln Builders
Kiln@Minn.net
----------
> From: john eden
> To: CLAYART@LSV.UKY.EDU
> Subject: Bricks, help
> Date: Tuesday, November 24, 1998 8:42 AM
>
> ----------------------------Original message----------------------------
> I would appreciate it if someone could give me details on the following
> bricks, maker, temp, etc..
>
> Firebrick "HI - HEAT"
> Firebrick "S - I DP
>
> Thanks in advance, cheers, John.
>
> John Eden
> Hudson, Quebec, J0P 1H0, Canada
> Tel. # 514-457-6610 ext. 395 (office)
> Tel. # 450-458-7097 (home)
> e-mail> john.eden@johnabbott.qc.ca
| |
|