search  current discussion  categories  glazes - cone 8-10 

crystaline glazes at cone 10 reduction

updated wed 2 sep 98

 

Scott Barnim on tue 1 sep 98

Six months ago I started a series of tests for Crystaline glazes at cone 10
in reduction. I didn't get to far before I was side tracked and I've been
thinking about were to go next with these tests. There are some
restrictions that I have imposed, I have a large kiln and the glaze tests,
and any eventual glaze has to fit into a standard reduction firing
schedule. has anyone out there had experience with this sort of persuit?

Scott Barnim BARNIM@INTERLYNX.NET
15 Park Street East, Dundas, Ontario. L9H1C9 (905) 628 2507