Elke Blodgett on fri 20 nov 98
---------- Forwarded message ----------
Date: Tue, 17 Nov 1998 17:49:06 -0500
From: Monona Rossol <75054.2542@compuserve.com>
Subject: Granola Fascism (fwd)
---------- Forwarded message ----------
Date: Mon, 16 Nov 1998 12:43:08 EST
From: Fay & Ralph Loewenthal
To: CLAYART@LSV.UKY.EDU
Subject: Granola Fascism (fwd)
----------------------------------------------
Reply to Ralph
Thanks for the kind words. One interesting point in your post I'd
like to comment on:
> I have been experimenting with Barytes (Barium Sulfate)
> to try and get the same colours, but no luck so far. Barytes
> is the gunk they feed you when you have a Barium Meal to
> find out if you have ulcers or not. I assume it is not toxic. <
T'ain't. But it can do some interesting things. If you inhale the dust it
essentially just sits in the lungs and does the same thing it does when you
get a barium meal: it makes your lungs opaque! Those fuzzy x-rays can hide
other diseases. And the doctors will probably kill you trying to find out
why your x-rays look like that!
And remember--whether you use the barium or the sulfate or the carbonate, in
the glaze, they are just barium. Both can leach.
Monona
ACTS
181 Thompson St., # 23
NYC NY 10012 212.777-0062
| |
|