DEBORAH K FERREE on wed 4 nov 98

I have the Gun Melal =5E6 Glaze for you. Works well on all clays. A nice =
satin
black. Also a nice metallic black under floating blue where it overlaps.

Gun Metal Albany =5E5-6

Gertley Borate 11.22
Albany Slip Clay (real or Sub) 88.78
Copper Carb 7.78