Emmanuel Cooper's The Potter's Book of Glaze Recipes has the following recipe listed for cone 5: Standard borax frit 85 =5BFerro 3134=5D china clay 15 red iron oxide 10=25 Is this the firing range you're looking for? Judi Buchanan