i tested the glazes in p.m.illust. winter/98

updated tue 3 nov 98

 

Amy Gossett on mon 2 nov 98

I just got through testing the glazes that were in the winter 98 issue of
Pottery Making Illustrated. The article was written by Sumi Von Dassow. I
really liked what I yielded and I am about to make up some larger samples to
test on some test-pots.

The glazes came out pretty darn close to what the pictures showed in the
magazine, with some variations that I wanted to change up a little=21 I =
thought
they were darn good considering I always screw up something in my =
calculations=21

If anyone else tried these...let me know...curious to see what other folks =
who
tried these came up with=21


Amy Gossett
Located in =22Peachy=22 Albany, Georgia alongside the Flint River.
=2A=2A=2ANOTE TO CLAYART DISCUSSIONS=2A=2A: When Responding to a post =
directly to
me...please include CLAYART in the subject line=21
CoolPotter=40worldnet.att.net
http://home.att.net/=7Ecoolpotter/welcome.html
AOL Instant Messenger: BADBEAMER

=22Television does not make a perfectly sane man go out and kill 5 people.
Not even =22must see TV=22.=22---Fox Mulder, The Xfiles