search  current discussion  categories  kilns & firing - cones & controllers 

kiln controllers & storms

updated fri 11 dec 98

 

L&L Kiln Mfg on thu 10 dec 98

At 10:18 PM 12/6/98 EST, you wrote:
>----------------------------Original message----------------------------
>
>
>The controls for the klin at my school went hay wire. We were having
>strong winds a week a go and the electrcity went out and now they're
>broken.
>(Moral of the story: Don't turn klins on in stormy weather.)
>Liz in Vancouver
>It's still windy
>
>______________________________________________________
>Get Your Private, Free Email at http://www.hotmail.com
>
We have been offering to our customers the option of having the power that
feeds the control panel be on a separate 120 volt line with an EMI noise
filter. They can then plug this line into a computer surge protector and
prevent death by lightning.
Stephen Lewicki
President
L&L Kiln Mfg Inc.
Phone: (610) 558-3899
Fax: (610) 558-3698
Email: steve@hotkilns.com