I'm getting ready to fire off my new gas kiln for the first time. I
misplaced my recipe for kiln wash that has a low amount of free silica.
Can anyone help? Veronica

David Hewitt on tue 29 sep 98

May I suggest that you just use Alumina Hydrate or Silca Sand. Just
sprinkle thinly on the kiln bats. It is easier and cleaner than kiln
wash.
In message , honthaas writes
>----------------------------Original message----------------------------
>I'm getting ready to fire off my new gas kiln for the first time. I
>misplaced my recipe for kiln wash that has a low amount of free silica.
>Can anyone help? Veronica
>

--
David Hewitt
David Hewitt Pottery ,
7 Fairfield Road, Caerleon, Newport,