search  current discussion  categories  forms - misc 

laguna rough bottoms

updated sun 16 aug 98

 

peacepttry on sat 15 aug 98

We've been having a problem for about the last two months where the bottom
of our pots are rougher than normal and require sanding where they didn't
before. It's only happening on Laguna's clay. ( Death Valley, Soldate and
Rod's Bod.) Our other bodies which aren't Laguna aren't reacting any
differently. We fire cone 10 reduction and the firing schedule is the same.
Anyone else having this problem? Any comments would be greatly appreciated.

Mindy & Greg
Peaceful Prairie pottery