Dai Scott on fri 18 sep 98
The post from Leslie about the cream/white glaze was scattered all over my
screen, with figures not lining up with chemicals. I have taken down the
recipe as follows (can someone let me know if this is right?):
Dolomite 21
Gerstley Borate 10
Spodumene 9
Wollastonite 5
Custerspar 27
Neph Sy 12
Kaolin 16
Thanks!
Dai Scott - Pottery by Dai
Kelowna, B.C. --still sorting thru the week's mail!
| |
|