What has worked for you in using low fire crackle glazes? I tried Amaco low
fire crackle glaze according to directions (apply three coats to a bisque
piece fired to cone 04 and then refired with the white crackle glaze to cone
010) and got a foam surface rather than crackle effects. My raku crackle
glaze works well for me in the raku process. Your help would be appreciated!