search  current discussion  categories  techniques - majolica 

maple satin glaze

updated fri 27 nov 98

 

Chris Schafale on thu 26 nov 98

Anyone out there familiar with a glaze called Maple Satin? It was
used at the community arts center where I used to work, and I can't
get the recipe, but I'd love to try to duplicate it. It fires a
soft greenish-tan and has a lovely matte surface so buttery you can
gain weight just looking at it. Fires to cone 6 in oxidation.
That's all I can tell you. Any ideas? Thanks in advance

Chris
Light One Candle Pottery
Fuquay-Varina, NC
candle@nuteknet.com