Lynn Koning on tue 12 jan 99

when I bisque my stoneware, it turns a pretty peach color. does anyone have a
^6-7 ox glaze recipe anywhere near a peach color? searched the archives and
can't find one. Thanks
Lynn Koning in L.A. (lower Alabama) where there's still ice in my birdbath at
noon.just doesn't seem right!

DinaH on thu 14 jan 99

Lynn
Susan Demay included this in her glaze recipes at NCECA 97. It looked good in th
test I did.
Peachy Keen ^6
Gerstley Bor 1224
Potash Felds 4140
Flint 1692
EPK 225
Whiting 729
Zircopax 540
Dolomite 540
Bentonite 90
Rutile 720

Dinah
Lynn Koning wrote:

> ----------------------------Original message----------------------------
> when I bisque my stoneware, it turns a pretty peach color. does anyone have a
> ^6-7 ox glaze recipe anywhere near a peach color? searched the archives and
> can't find one. Thanks
> Lynn Koning in L.A. (lower Alabama) where there's still ice in my birdbath at
> noon.just doesn't seem right!