problems with glaze

updated fri 8 jan 99

 

Alex Wilson on thu 7 jan 99

Hello Mathew,
The only thing I can think of, is to make sure you are putting your glaze
through a fine enough lawn as the frits *may* have some granular content. 100s
to 150s should do it. Try examining the bumps with a magnifying lens to see if
it is a material problem.
Good luck,
Alex